    Effect of Storage Media and Sterilization Method on Shear Bond Strength of Composite to Enamel of Extracted Teeth

    (ندگان)پدیدآور
    Boruziniat, AlirezaDanaifard, NasrinGifani, MahshidHakimi, Narjes
    Thumbnail
    دریافت مدرک مشاهده
    FullText
    اندازه فایل: 
    353.0کیلوبایت
    نوع فايل (MIME): 
    PDF
    نوع مدرک
    Text
    Original Article
    زبان مدرک
    English
    نمایش کامل رکورد
    چکیده
    Aim: To evaluate the effect of storage media and autoclaving on shear bond strength of composite to enamel. Materials and Methods: 100 human premolars were randomly divided into ten groups of ten as follows: C: freshly extracted teeth. A: Autoclaved freshly extracted teeth. CH-6: 6 month storage in 0.5 % chloramine T. CA-6: 6 month storage in 0.5 % chloramine T + autoclaving. T-6: 6 month storage in 0.04 % thymol. TA-6: 6 month storage in 0.4% thymol + autoclaving. Ch-12:12 month storage in 0.5 % chloramine T. CA-12: 12 month storage in 0.5 % chloramine T + autoclaving. T-12: 12 month storage in 0.4% thymol. TA-12:12 month storage in 0.4% thymol + autoclaving. One composite cylinder was bonded on each specimen for evaluation of shear bond strength (SBS) and failure modes. Data were analyzed using three-way ANOVA, Tukey's post hoc and Chi square tests and the level of significance was set  at P= 0.05. Results: Autoclaving and storage media had no significant effect on SBS (P-value = 0.818 for storage media and P-value = 0.221 for autoclaving). However, storage duration significantly changed SBS (P-value = 0.00). There were no correlations among the variables (P-value > 0.05). Storage media and duration had no significant effect on failure modes (P-value > 0.05), but autoclaving significantly increased cohesive failure of enamel (P-value =0.039). 0.05). Storage media and duration had no significant effect on failure modes (P-value > 0.05), but autoclaving significantly increased cohesive failure of enamel (P-value =0.039). 0.05), but autoclaving significantly increased cohesive failure of enamel (P-value =0.039). Conclusion: Storage of teeth in chloramine T and thymol had no significant effect on bond strength to enamel. Although autoclaving of specimens may not alter bond strength, it can significantly increase the cohesive failure of enamel.  
    کلید واژگان
    Autoclaving
    Bond Strength
    chloramine T
    extracted teeth
    storage media
    Thymol
    Operative Dentistry

    شماره نشریه
    3
    تاریخ نشر
    2017-09-01
    1396-06-10
    ناشر
    Mashhad University of Medical Sciences
    سازمان پدید آورنده
    Dental Materials Research Center, School of Dentistry, Mashhad University of Medical Sciences, Mashhad, Iran
    general dentist
    Post-graduate student, Department of Pediatric Dentistry, School of Dentistry, Mashhad University of Medical Sciences, Mashhad, Iran
    Post-graduate student, Department of Operative Dentistry, School of Dentistry, Mashhad University of Medical Sciences, Mashhad, Iran

    شاپا
    2322-4150
    2252-0317
    URI
    https://dx.doi.org/10.22038/jdmt.2017.9012
    http://jdmt.mums.ac.ir/article_9012.html
    https://iranjournals.nlai.ir/handle/123456789/280167

    مرور

    همه جای سامانهپایگاه‌ها و مجموعه‌ها بر اساس تاریخ انتشارپدیدآورانعناوینموضوع‌‌هااین مجموعه بر اساس تاریخ انتشارپدیدآورانعناوینموضوع‌‌ها

    حساب من

    ورود به سامانهثبت نام

    آمار

    مشاهده آمار استفاده

    تازه ترین ها

    تازه ترین مدارک
    © کليه حقوق اين سامانه برای سازمان اسناد و کتابخانه ملی ایران محفوظ است
    تماس با ما | ارسال بازخورد
    قدرت یافته توسطسیناوب