Optimized Leaching Conditions for Selenium from Sar-Cheshmeh Copper Anode Slimes
(ندگان)پدیدآور
Abdollahy, MahmoudShafaei, Seid Ziadinنوع مدرک
TextResearch Article
زبان مدرک
Englishچکیده
The recovery process of selenium from Iranian Sar-Cheshmeh copper anode slimes employing hydrometallurgical methods has been investigated. The copper anode slimes are made up of those components of the anodes, which are not soluble in the electrolyte. They contain varying quantities of precious metals like gold, silver, selenium and tellurium. They are being extracted as a by product in the copper production process.In this paper, some parameters affecting the leaching conditions of anode slimes in nitric acid are studied. Taguchi experimental design method is used to find out the effect of acid concentration, temperature and time.The statistical results of the experiments show that the above parameters are important in the leaching of -10 microns fraction. The optimum conditions determined are: T = 90º C, acidity = 4 M and the leaching time = 60 min. Under these conditions, 99 % of the selenium is leached out.
کلید واژگان
Sar-Cheshmeh mineCopper anode slimes
Hydrometallurgy
Selenium extraction
Ore Dressing, Mineral Processing
شماره نشریه
2تاریخ نشر
2004-12-011383-09-11
ناشر
Iranian Institute of Research and Development in Chemical Industries (IRDCI)-ACECRسازمان پدید آورنده
Mineral Processing Group, Tarbiat Modarres University, P.O. Box 14115-143, Tehran, I.R. IRANMining Department, Technical University of Shahrood, Shahrood, I.R. IRAN