      Comparison Of Chlorhexidine 2% And Sodium Hypochlorite 5% As Rewetting Agents On Resin- Dentin Micro Tensile Bond Strength

      (ندگان)پدیدآور
      Karrabi, MaliheDavari, Abdol rahimDanesh Kazemi, Alireza
      Thumbnail
      دریافت مدرک مشاهده
      FullText
      اندازه فایل: 
      284.2کیلوبایت
      نوع فايل (MIME): 
      PDF
      نوع مدرک
      Text
      Original Article
      زبان مدرک
      English
      نمایش کامل رکورد
      چکیده
      Resin- dentin interface hydrolysis is one of the greatest problems in restorative dentistry, Because of collagenolytic and proteolytic activity of dentin enzymes. The aim of this study was to compare the effect of CHX 2% and NaOCl 5% as rewetting agent on resin-dentin micro tensile bond strength.Methods: 45 extracted, human caries-free third molar teeth were collected. After exposing of superficial dentin, etching and rinsing of dentin were done. Specimens were divided into 3 equal groups. In group 1, after drying of dentin, CHX 2% was used as rewetting agent for 60 seconds. In group2, NaOCl 5% used as rewetting agent for 120 sec and in group 3 (control), blot dry technique with water was used for substrate. Adhesive system (SingleBond , 3M ESPE , USA) and composite build up (Filtek Z250 ,3M ESPE , USA)) were applied for all groups. After 6 month storage, μTBS measured for hourglass-shaped specimens. Specimens loaded for micro tensile bond strength until fracture occurred. Results: Micro tensile bond strength of group 1 significantly was higher than other groups (52.67±6.862). There was no significant difference between group 2(18.59 ± 6.081) and group 3(28.84± 6.231). (P= 0.094).  Conclusion: CHX acts as matrix metalloproteinases inhibitor and by preventing dentin collagen degradation can preserve the bond strength after 6 months.
      کلید واژگان
      Dentin
      micro tensile bond strength
      CHX
      matrix metalloproteinases inhibitor
      Dentistry
      Operative Dentistry

      شماره نشریه
      4
      تاریخ نشر
      2016-12-01
      1395-09-11
      ناشر
      Mashhad University of Medical Sciences
      سازمان پدید آورنده
      Assistant Professor, Department of Operative Dentistry, School of Dentistry, Gilan University of Medical Sciences, Gilan, Iran
      Professor, Department of Operative Dentistry, Social Determinants of Oral Health Research Center, Dental School, Shahid Sadoughi University of Medical Sciences, Yazd, Iran
      Associated Professor, Department of Operative Dentistry, Social Determinants of Oral Health Research Center, Dental School, Shahid Sadoughi University of Medical Sciences, Yazd, Iran

      شاپا
      2322-4150
      2252-0317
      URI
      https://dx.doi.org/10.22038/jdmt.2016.7617
      http://jdmt.mums.ac.ir/article_7617.html
      https://iranjournals.nlai.ir/handle/123456789/280259

      مرور

      همه جای سامانهپایگاه‌ها و مجموعه‌ها بر اساس تاریخ انتشارپدیدآورانعناوینموضوع‌‌هااین مجموعه بر اساس تاریخ انتشارپدیدآورانعناوینموضوع‌‌ها

      حساب من

      ورود به سامانهثبت نام

      تازه ترین ها

      تازه ترین مدارک
      © کليه حقوق اين سامانه برای سازمان اسناد و کتابخانه ملی ایران محفوظ است
      تماس با ما | ارسال بازخورد
      قدرت یافته توسطسیناوب