Bioleaching of Low Grade Uranium Ore of Saghand Mine
(ندگان)پدیدآور
Abdollahy, MahmoudShojaosadati, Sayed AbbasZare Tavakoli, HasanValivand, Aliنوع مدرک
TextResearch Note
زبان مدرک
Englishچکیده
This study deals with bioleaching of the low grade uranium ore of Saghand mine in Iran using a mixed culture of mesophilic bacteria (Acidithiobacillus ferrooxidans, Acidithiobacillus thiooxidans and Leptospirillum ferrooxidans). Experiments were carried out in shaking flask examining the effect of temperature, initial ferrous ion concentration, pulp density and particle size. Variations of pH, Eh, ferrous ion concentration, cells growth and uranium extraction were monitored. The highest rates of leaching and extraction were obtained at 35ºC, 2.5% (w/v) pulp density, 4 g/l ferrous ion and - 106µm particle size.
کلید واژگان
BioleachingMesophilic bacteria
Uranium ore
Biotechnology
Ore Dressing, Mineral Processing
شماره نشریه
4تاریخ نشر
2011-12-011390-09-10
ناشر
Iranian Institute of Research and Development in Chemical Industries (IRDCI)-ACECRسازمان پدید آورنده
ineral Processing Group, Faculty of Engineering, Tarbiat Modares University, Tehran, I.R. IRANBiotechnology Group, Faculty of Engineering, Tarbiat modares University, Tehran, I.R. IRAN
Mineral Processing Group, Faculty of Engineering, Tarbiat Modares University, Tehran, I.R. IRAN
EMKA Company, Iran Atomic Energy Organization, Tehran, I.R. IRAN