Preparation and characterization of fluorapatite-bioactive glass S53P4 nanocomposite
(ندگان)پدیدآور
Manafi, SahebaliMirjalili, FatemehHajisafari, MahmoodOrand, Faranakنوع مدرک
TextOriginal Research Paper
زبان مدرک
Englishچکیده
This research has been done to study characteristic and biocompatible evaluation of a nano-biocompositeceramic with the bioglass (BG) as a first phase. In this regard, synthesis of S53P4 (53% SiO2, 4% P2O5,23% Na2O and 20% CaO) bioglass has been considered as the first phase and flourapatite (FA) consideredas the second phase. Afterwards, nanocomposite with the base of S53P4 bioglass has been synthesizedby sol-gel method. The synthesized nanoparticles and nanocomposite have been characterized with thehelp of different techniques, using field emission scanning electron microscope (FESEM), X-ray diffraction(XRD), Fourier transforms infrared spectroscopy (FT-IR), X-ray fluorescence (XRF) to evaluate crystalstructure, microstructure, and morphology. The results showed that the crystallite size and the crystallinityof S53P4 bioglass-fluorapatite nanocomposites were about 20-30 nm and 70-90%, respectively.The FT-IR analyses displayed that the purity in the structure of this nanocomposite. The result of MTT(3-(4,5-Dimethylthiazol-2-Yl)-2,5-Diphenyltetrazolium Bromide) assay indicated the nontoxicity and alsodecreasing of cell viability in 7 days compared with the first day.
کلید واژگان
BiocompatibleBioglass
Fluorapatite
MTT Assay
S53P4
شماره نشریه
3تاریخ نشر
2019-09-011398-06-10
ناشر
Tehran Medical Sciences, Islamic Azad University, Tehran, Iranسازمان پدید آورنده
Department of Engineering, Shahrood Branch, Islamic Azad University, Shahrood, IranDepartment of Material Engineering, Maybod Branch, Islamic Azad University, Maybod, Iran
Department of Material Engineering, Yazd Branch, Islamic Azad University, Yazd, Iran
Department of Material Engineering, Yazd Branch, Islamic Azad University, Yazd, Iran