Studies on the SPEEK membrane with low degree of sulfonation as a stable proton exchange membrane for fuel cell applications
(ندگان)پدیدآور
Parnian, Mohammad JavadGashoul, FatemehRowshanzamir, Soosanنوع مدرک
TextResearch Paper
زبان مدرک
Englishچکیده
Sulfonated poly (ether ether ketone) (SPEEK) with a low degree of sulfonation (DS = 40%) was prepared for proton exchange membrane fuel cells (PEMFC). Poly (ether ether ketone) (PEEK) was sulfonated in concentrated H2SO4 under N2 atmosphere and characterized by the hydrogen nuclear magnetic resonance (H-NMR) technique. After preparation of the SPEEK polymer, the obtained polymer was dissolved in dimethylacetamide (DMAC) solvent and then the solution casting method was applied for the fabrication of membranes. Water uptake behavior, ion exchange capacity (IEC), and the proton conductivity at different temperatures and different relative humidity were determined and compared with a commercial Nafion 117 membrane. The IEC and the proton conductivity results showed that the sulfonation process successfully created proton conduction channels. In addition, the thermal, mechanical, chemical, and hydrolytic stabilities were thoroughly investigated for the prepared membrane. The low degree of sulfonation SPEEK showed a desirable chemical durability with a higher dimensional, mechanical, and thermal stability than Nafion-117 but lower water uptake and proton conductivity.
کلید واژگان
Proton exchange membraneSPEEK
fuel cell
stability
Chemical Engineering
شماره نشریه
3تاریخ نشر
2016-08-011395-05-11
ناشر
Iranian Research Organization for Science and Technologyسازمان پدید آورنده
School of Chemical Engineering, Iran University of Science and Technology, Narmak, Tehran 16846-13114, IranSchool of Chemical Engineering, Iran University of Science and Technology, Narmak, Tehran 16846-13114, Iran
Green Research Center (GRC) & School of Chemical Engineering (SChE) Iran University of Science & Technology
شاپا
2383-160X2383-1618