نمایش مختصر رکورد

dc.contributor.authorBahrami Alamdarlo, Masouden_US
dc.contributor.authorAmini, Kamranen_US
dc.contributor.authorNemati Najafabadi, Vahiden_US
dc.contributor.authorMohammadnezhad, Mahyaren_US
dc.date.accessioned1399-07-08T23:50:09Zfa_IR
dc.date.accessioned2020-09-29T23:50:09Z
dc.date.available1399-07-08T23:50:09Zfa_IR
dc.date.available2020-09-29T23:50:09Z
dc.date.issued2016-03-01en_US
dc.date.issued1394-12-11fa_IR
dc.date.submitted2016-03-11en_US
dc.date.submitted1394-12-21fa_IR
dc.identifier.citationBahrami Alamdarlo, Masoud, Amini, Kamran, Nemati Najafabadi, Vahid, Mohammadnezhad, Mahyar. (2016). Investigating the Effect of Titanium Addition on the Microstructure and Mechanical Properties of Ni-Hard 4 Cast Iron. Journal of Modern Processes in Manufacturing and Production, 5(1), 17-27.en_US
dc.identifier.issn2717-0314
dc.identifier.issn2717-0322
dc.identifier.urihttp://mpmpjournal.iaun.ac.ir/article_560027.html
dc.identifier.urihttps://iranjournals.nlai.ir/handle/123456789/163669
dc.description.abstractNi-Hard4 white cast iron is excellent wear resistant material and has been widely used in wearaffected equipment operated under extreme conditions, such as in mineral processing, cement, copper and iron manufacturing. In this study the effect of titanium addition (1.2, 0.7 and 0.2 wt.%) to the Ni-hard 4 cast iron with the nominal composition of Si= 1.5%, Mn=0.5%, C=3%, P=0.05%, S= 0.05%, Mo= 0.1%, Cr= 8% and Ni= 5.5% was investigated. This study was focused on the hardness, tensile strength, wear resistance and microstructural changes of the Ni-hard 4 cast iron. The results were compared with the Ni-hard 4 titanium free cast iron and demonstrated that the carbide morphology changes from rough plane to the flower leaf due to titanium addition. In addition, results showed that by increasing the percentage of titanium, hardness, strength and wear resistance is improved. In the samples with 1.3% titanium, the hardness, strength and wear resistance improved for 35, 22.5 and 85% respectively as compared with the titanium-free samples. This behavior is a consequence of the chromium carbide replacement with the hard titanium carbides as well as grain refining. Investigating the worn out surface of the samples showed that the predominant wear mechanism is the combination of the adhesive and tibo-chemical.en_US
dc.format.extent1348
dc.format.mimetypeapplication/pdf
dc.languageEnglish
dc.language.isoen_US
dc.publisherIslamic Azad Univesity, Najafabad Branchen_US
dc.relation.ispartofJournal of Modern Processes in Manufacturing and Productionen_US
dc.subjectNi-Hard 4 Cast Ironen_US
dc.subjectTitanium Carbideen_US
dc.subjectWear resistanceen_US
dc.subjectHardnessen_US
dc.titleInvestigating the Effect of Titanium Addition on the Microstructure and Mechanical Properties of Ni-Hard 4 Cast Ironen_US
dc.typeTexten_US
dc.contributor.departmentYoung Researchers and Elite Club, Najafabad Branch, Islamic Azad University, Najafabad, Iranen_US
dc.contributor.departmentDepartment of Mechanical Engineering, Tiran Branch, Islamic Azad University, Isfahan, Iranen_US
dc.contributor.departmentYoung Researchers and Elite Club, Najafabad Branch, Islamic Azad University, Najafabad, Iranen_US
dc.contributor.departmentDepartment of Materials Engineering, Isfahan University of Technology, Isfahan, Iranen_US
dc.citation.volume5
dc.citation.issue1
dc.citation.spage17
dc.citation.epage27